Last weekend I continued as planned by giving the interior a final sand, vacuum and wipe down. Satisfied that I had as perfect a surface as possible, I happily threw myself at laminating the first strip amidships. I was pretty confident, since the test panel had turned out brilliantly.

The initial coat of epoxy went on easily enough, but when I attempted to apply the strip of fiber glass cloth, all of the horrors from my earlier laminating of the hull's exterior came flooding back. The cloth would pull this way and that. Folds would develop in one place, and once sorted out, the cloth suddenly wouldn't reach the gunwales anymore. I'd fiddle around and swear at it until it eventually seemed to behave itself, when suddenly one of the clamps would fly off and a great fold of cloth would peel away from the surface, forcing me to start all over again. I tried to use the peel-ply, thinking that it might help to tame the unruly glass cloth, but it only made matters worse. The wispy light fabric of the peel-ply took on characteristics similar to normal glass cloth on crystal-meth., and when it got near it's partner in crime, they appeared to rejoice in an orgy of mischief. After wrestling with these two evil materials for some time, I decided to abandon the peel-ply and concentrated my fight solely on the glass cloth (divide and conquer). Somehow, I finally managed to force it into some semblance of order. This process took so long (and taxed my mental/emotional faculties so much), that I couldn't get any further that day. This photo shows the result. Slightly less ideal than my test panel, but should be ok.
(Score, Me:1 - Glass Cloth: nil)







The next day, I warily approached the canoe with a mixture of respect and disgust, but also determination. This bastard wasn't going to beat me. This time I was going to take it easy, work strategically and show no signs of weakness. It was going to be a hot day, but dry. I thought about trying to string up a tarp, but because I wanted to come to grips with my enemy quickly, I instead decided to attack straight away.

This time, so as to ensure absolute control of this mongrel fabric, I opted to use the 'dry method' of laminating. This means not applying an initial layer of epoxy first, then laying the cloth over this, followed by applying subsequent applications of epoxy (aka; 'wet method'). By using the dry method, I intended to clamp the recalcitrant glass cloth in place, whilst slowly and methodically assaulting it with the epoxy. This seemed to work pretty well. The glass cloth did make a couple of feints and counter attacks, but through effective flanking maneuvers and by maintaining a steely focus, I finally emerged victorious. Feeling quite proud of myself, I bowed smugly to my foe and retired for the day (it was pretty hot, after all).

At the end of the day I came back to cover up the hull for the night and discovered a slight flaw to my tactics. By leaving the wet lamination in the direct sun (something which pretty much everybody says not to do - and in hindsight seems pretty dumb anyway), the surface must have heated up too much, causing air to bubble up from the surface. This left lots of big blisters, which I'm now going to have to sort out.
(Score, 1 - all)




The next time, I decided to learn from my mistake. I dug out my army hootchie (cammo fly-sheet) and strung it up over the next section with occy-straps. Then I proceeded with the same clamping/dry technique that seemed to work so well before.



This time I was much more successful. This is more like it, although I still loath fiber-glassing.
(Score, Me: 2 - Glass Cloth: 1)






The next day, I assaulted the bow section. With my trusty hootchie in place again, I followed Gary's advice about laminating each side separately, and applying a strip to cover the join. A bit fiddly, and the cloth still tried the odd rebellion here and there, but overall it worked very well.
(Score, Me: 3 - Glass Cloth: 1)









Today it was the stern section's turn to get laminated. Same again, another victory.
(Game, Set and Match, bitch!)






So I now have the whole interior initially laminated. There's a little bit of rework yet to be done on the blisters, and the whole lot needs a decent fill coat of epoxy to cover up the stitching of the cloth, which is still sitting proud of the surface. I'm wondering if I might be able to use the pee-ply on this fill coat, so I don't end up using too much epoxy. Reckon I might give Pacific Boatcraft a call tomorrow and ask them. Hopefully I'd be able to tame that foul fabric as well (bring it on).